General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Water absorption | 23.0 °C | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ISO 527 | yield, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 90 MPa Show Supplier Material materials with Flexural strength of 90 MPa | ISO 178 | yield, 2 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Charpy notched | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 60 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C | ||
Impact strength, Izod notched | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 60 kJ/m² | ISO 180/1A | 80*10*3, 23°C | ||
Tensile strength | 23.0 °C | 63 MPa Show Supplier Material materials with Tensile strength of 63 MPa | ISO 527 | yield, 50 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | 80*10*3, 23°C |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Heat deflection temperature | 121 - 133 °C Show Supplier Material materials with Heat deflection temperature of 121 - 133 °C | ||
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Vicat softening temperature | 139 °C Show Supplier Material materials with Vicat softening temperature of 139 °C | ISO 306 | Rate B/50 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 275 V Show Supplier Material materials with Comparative tracking index of 275 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 26 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 26 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Management, Audio, Circuit Protection, LED Lighting, Personal Computing, Non-LED Lighting, Rear/Signal Lighting | |
Availability | Europe | |
Processing methods | Middle - Zone 2 Temperature: 270 to 290.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |