General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 31.4 GPa Show Supplier Material materials with Elastic modulus of 31.4 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 6.7 % Show Supplier Material materials with Elongation of 6.7 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Flexural modulus of 3.2 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 82 MPa Show Supplier Material materials with Flexural strength of 82 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 48 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 48 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 62 MPa Show Supplier Material materials with Tensile strength of 62 MPa | ASTM D 638 | break |
Thermal
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 2 % Show Supplier Material materials with Shrinkage of 2 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling | |
Availability | Europe,Americas | |
Processing methods | Rear - Zone 1 Temperature: 175 to 190.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |