General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Density of 1.29 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.29 [-] Show Supplier Material materials with Relative density of 1.29 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 1.03 % Show Supplier Material materials with Water absorption of 1.03 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 3.3 GPa Show Supplier Material materials with Elastic modulus of 3.3 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 54 % Show Supplier Material materials with Elongation of 54 % | ISO 527 | break, 5 mm/min | ||
Flexural modulus | 23.0 °C | 3.1 GPa Show Supplier Material materials with Flexural modulus of 3.1 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 170 MPa Show Supplier Material materials with Flexural strength of 170 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span | ||
Impact strength, Charpy notched | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C | ||
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 37 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 37 J/m | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2440 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2440 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 33 J Show Supplier Material materials with Instrumented Impact, Total Energy of 33 J | ASTM D 3763 | 23°C | ||
Tensile strength | 23.0 °C | 103 MPa Show Supplier Material materials with Tensile strength of 103 MPa | ISO 527 | yield, 5 mm/min | ||
Impact strength, Izod unnotched | ISO 180/1U | 80*10*4, 23°C |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Heat deflection temperature | 196 - 215 °C Show Supplier Material materials with Heat deflection temperature of 196 - 215 °C | ||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 196 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 196 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Vicat softening temperature | 221 °C Show Supplier Material materials with Vicat softening temperature of 221 °C | ISO 306 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 11 g/10min Show Supplier Material materials with Melt mass-flow rate of 11 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Melt volume-flow rate | 16 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 16 cm³/10min | ISO 1133 | MVR at 360°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Fog Lamp | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |