General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 76 % Show Supplier Material materials with Elongation of 76 % | SABIC - Japan Method | break |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 75 MPa Show Supplier Material materials with Flexural strength of 75 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 236 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 236 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 236 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 236 J/m | ASTM D 256 |
Tensile strength | 23.0 °C | 44 MPa Show Supplier Material materials with Tensile strength of 44 MPa | SABIC - Japan Method | yield |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | TMA | -30°C to 30°C |
Heat deflection temperature | 120 °C Show Supplier Material materials with Heat deflection temperature of 120 °C | ||
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 6.4 mm, unannealed |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 6.6 g/10min Show Supplier Material materials with Melt mass-flow rate of 6.6 g/10min | ASTM D 1238 | 250°C/10.0 kgf | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Availability | Asia | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |