General
Property | Temperature | Value | Comment |
---|---|---|---|
Moisture absorption | 23.0 °C | 0.02 % Show Supplier Material materials with Moisture absorption of 0.02 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.1 [-] Show Supplier Material materials with Relative density of 1.1 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.13 % Show Supplier Material materials with Water absorption of 0.13 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 3.1 GPa Show Supplier Material materials with Elastic modulus of 3.1 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 7.3 % Show Supplier Material materials with Elongation of 7.3 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.8 GPa Show Supplier Material materials with Flexural modulus of 2.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 98 MPa Show Supplier Material materials with Flexural strength of 98 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Tensile strength | 23.0 °C | 52 MPa Show Supplier Material materials with Tensile strength of 52 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.4E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+14 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+14 Ω | IEC 60093 |
Volume resistivity | 23.0 °C | 4.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 4.00E+16 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 34 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 34 cm³/10min | ISO 1133 | MVR at 280°C/2.16 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Displays, Washing Machine | |
Availability | Europe | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |