General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.12 % Show Supplier Material materials with Water absorption of 0.12 % | ISO 62-1 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 6 GPa Show Supplier Material materials with Elastic modulus of 6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.5 % Show Supplier Material materials with Elongation of 2.5 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 5.4 GPa Show Supplier Material materials with Flexural modulus of 5.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 167 MPa Show Supplier Material materials with Flexural strength of 167 MPa | ISO 178 | yield, 2 mm/min |
Tensile strength | 23.0 °C | 97 MPa Show Supplier Material materials with Tensile strength of 97 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature | 137 °C Show Supplier Material materials with Heat deflection temperature of 137 °C | ||||
Heat deflection temperature, 1.80 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 137 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 90 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |||
Vicat softening temperature | 146 °C Show Supplier Material materials with Vicat softening temperature of 146 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228545- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237020- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 15 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 15 cm³/10min | ISO 1133 | MVR at 280°C/10.0 kg | |
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Enclosure/Housing/Cover, Energy Management, Electronic Components, Hot Water System, Heavy Vehicles, Industrial Material Handling, Lawn/Garden, Lab Ware and Clinical Diagnostics, Fixture Bath/Shower, Food Processor, Food Container, Freezer, Food Transportation, Exterior Mirror, Engine Component, Coffee Maker/Espresso Machine, Bottles, Data Transfer, Data Management, Dishwasher, Dunnage, Displays, Document Handling, Auto Aftermarket, Audio, Animal Testing, Circuit Protection, Building Accessory, Auto Electrical, Air Conditioning, Meter Water, Monitoring and Imaging, Ignition System, Meter Gas, Medical Device, Personal Computing, Motorcycle, Oil/Gas, Non-LED Lighting, Small Appliance, Semiconductor, Security/Detection, Pharmaceutical Packaging & Drug Delivery, Plumbing, Power Manangement, Pump, Pipe/Fitting, Recreational Vehicle, Water Treatment/Filtration, Weaving Machine, Wiring Devices, Wireless Communications, Vending Machine, Washing Machine, Tray, Vacuum Cleaner, Swimming Pool/Spa, Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |