Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1.2 GPa Show Supplier Material materials with Elastic modulus of 1.2 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 120 % Show Supplier Material materials with Elongation of 120 % | ASTM D 638 | brk, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 1.3 GPa Show Supplier Material materials with Flexural modulus of 1.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 49 MPa Show Supplier Material materials with Flexural strength of 49 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 587 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 587 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 33 MPa Show Supplier Material materials with Tensile strength of 33 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermal
Property | Value | Comment |
---|---|---|
Heat deflection temperature | 85 - 112 °C Show Supplier Material materials with Heat deflection temperature of 85 - 112 °C | |
Heat deflection temperature, 0.45 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 112 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C | ASTM D 648 | 3.2mm, unannealed |
Vicat softening temperature | 85 °C Show Supplier Material materials with Vicat softening temperature of 85 °C | ASTM D 1525 | Rate B/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Long Distance Coach, Recreational Vehicle | |
Availability | Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |