General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.71 g/cm³ Show Supplier Material materials with Density of 1.71 g/cm³ | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 22.4 GPa Show Supplier Material materials with Elastic modulus of 22.4 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 2.4 % Show Supplier Material materials with Elongation of 2.4 % | ASTM D 638 | break |
Flexural modulus | 23.0 °C | 19.4 GPa Show Supplier Material materials with Flexural modulus of 19.4 GPa | ASTM D 790 |
Flexural strength | 23.0 °C | 365 MPa Show Supplier Material materials with Flexural strength of 365 MPa | ASTM D 790 |
Impact strength, Izod notched | 23.0 °C | 170 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 170 kJ/m² | ASTM D 256 | notched, 23°C |
Tensile strength | 23.0 °C | 210 MPa Show Supplier Material materials with Tensile strength of 210 MPa | ASTM D 638 | break |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 210 °C Show Supplier Material materials with Heat deflection temperature of 210 °C | ||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |
Flammability | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093414- - |
Technological properties
Property | ||
---|---|---|
Application areas | Washing Machine, Wiring Devices | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |