General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.09 - 0.23 [-] Show Supplier Material materials with Coefficient of friction of 0.09 - 0.23 [-] | ||
Coefficient of friction, kinetic | 0.23 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.23 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.09 [-] Show Supplier Material materials with Coefficient of friction, static of 0.09 [-] | ASTM D 3702 Modified: Manual | |
Moisture absorption | 23.0 °C | 0.4 % Show Supplier Material materials with Moisture absorption of 0.4 % | ISO 62 | (23°C / 50% RH) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 9.4 % Show Supplier Material materials with Elongation of 9.4 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 2.9 GPa Show Supplier Material materials with Flexural modulus of 2.9 GPa | ISO 178 |
Flexural strength | 23.0 °C | 86 MPa Show Supplier Material materials with Flexural strength of 86 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 4 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 4 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 46 MPa Show Supplier Material materials with Tensile strength of 46 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 98 °C Show Supplier Material materials with Heat deflection temperature of 98 °C | ||
Heat deflection temperature, 1.80 MPa | 98 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 98 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101281603- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343834- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 2 % Show Supplier Material materials with Shrinkage of 2 % | ISO 294 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Delivery, EV Infrastructure, Lab Ware and Clinical Diagnostics, Enclosures, Electronic Components, Door Handle, Document Handling, ATM/Ticket Machine, Auto Electrical, LED Lighting, Personal Computing, Wireless Communications, Wearables | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |