General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.11 % Show Supplier Material materials with Water absorption of 0.11 % | ASTM D 570 | (23°C/24hrs) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1.2 % Show Supplier Material materials with Elongation of 1.2 % | ASTM D 638 | brk, Type I, 5 mm/min |
Flexural modulus | 23.0 °C | 8.8 GPa Show Supplier Material materials with Flexural modulus of 8.8 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Flexural strength | 23.0 °C | 113 MPa Show Supplier Material materials with Flexural strength of 113 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Taber Abrasion | 23.0 °C | 33 mg/1000cy Show Supplier Material materials with Taber Abrasion of 33 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Tensile strength | 23.0 °C | 82 MPa Show Supplier Material materials with Tensile strength of 82 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.62E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature | 212 °C Show Supplier Material materials with Heat deflection temperature of 212 °C | ||||
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 233 °C Show Supplier Material materials with Vicat softening temperature of 233 °C | ASTM D 1525 | Rate B/50 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221109- - <br> UL Recognized, 94V-0 Flame Class Rating: 0.84mm UL 94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.1 % Show Supplier Material materials with Shrinkage of 0.1 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosure/Housing/Cover, Enclosures, Circuit Protection, Wireless Communications, Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 135°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |