General
Property | Temperature | Value | Comment |
---|---|---|---|
Water absorption | 23.0 °C | 0.7 % Show Supplier Material materials with Water absorption of 0.7 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 1 % Show Supplier Material materials with Elongation of 1 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 7 GPa Show Supplier Material materials with Flexural modulus of 7 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 120 MPa Show Supplier Material materials with Flexural strength of 120 MPa | ISO 178 | break, 2 mm/min |
Taber Abrasion | 23.0 °C | 30 mg/1000cy Show Supplier Material materials with Taber Abrasion of 30 mg/1000cy | SABIC method | CS-17, 1 kg |
Tensile strength | 23.0 °C | 90 MPa Show Supplier Material materials with Tensile strength of 90 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ||||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 215 °C Show Supplier Material materials with Vicat softening temperature of 215 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: 0.84mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221109- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 4 V Show Supplier Material materials with Comparative tracking index of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosure/Housing/Cover, Enclosures, Circuit Protection, Wireless Communications, Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Hopper Temperature: 80 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |