General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Density of 1.09 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 34 % Show Supplier Material materials with Limiting oxygen index of 34 % | |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Water absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Water absorption of 0.15 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastic modulus of 2.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.4 GPa Show Supplier Material materials with Flexural modulus of 2.4 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 98 MPa Show Supplier Material materials with Flexural strength of 98 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 26 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Impact strength, Izod notched | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 9 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Tensile strength | 23.0 °C | 64 MPa Show Supplier Material materials with Tensile strength of 64 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Pass | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 8.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8.2E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 9.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9.4E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature | 114 - 129 °C Show Supplier Material materials with Heat deflection temperature of 114 - 129 °C | ||||
Heat deflection temperature, 0.45 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 129 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 114 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 114 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Vicat softening temperature | 149 °C Show Supplier Material materials with Vicat softening temperature of 149 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94V-1 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100158340- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.6 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 46 kV/mm Show Supplier Material materials with Dielectric strength of 46 kV/mm | IEC 60243-1 | shorttime, 1.0mm |
Dissipation factor, 1MHz | 23.0 °C | 1.7E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1.7E-3 [-] | IEC 60250 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt volume-flow rate | 9 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe/Fitting, Enclosures | |
Availability | Europe | |
Processing methods | Drying Time: 2 to 3.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |