General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 0.8 GPa Show Supplier Material materials with Elastic modulus of 0.8 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 4.5 % Show Supplier Material materials with Elongation of 4.5 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 85 MPa Show Supplier Material materials with Flexural strength of 85 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 20 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 202 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 202 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, at Peak | 23.0 °C | 40 J Show Supplier Material materials with Instrumented Impact, at Peak of 40 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 60 MPa Show Supplier Material materials with Tensile strength of 60 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature | 148 - 185 °C Show Supplier Material materials with Heat deflection temperature of 148 - 185 °C | ||||
Heat deflection temperature, 0.45 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 185 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 148 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 148 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Thermal conductivity | 23.0 °C | 0.25 W/(m·K) Show Supplier Material materials with Thermal conductivity of 0.25 W/(m·K) | ASTM C177 | ||
Vicat softening temperature | 190 °C Show Supplier Material materials with Vicat softening temperature of 190 °C | ISO 306 | Rate B/50 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: 1.2mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102297328- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 45 g/10min Show Supplier Material materials with Melt mass-flow rate of 45 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Melt volume-flow rate | 5 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 5 cm³/10min | ISO 1133 | MVR at 280°C/1.2 kg | |
Shrinkage | 23.0 °C | 1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 1 % Show Supplier Material materials with Shrinkage, transverse of 1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Sensor, Wheel Cover, Transmission/Transfer Comp, Traction Motor, Auto Electrical, Electronic Components, Heavy Vehicles | |
Availability | Asia,Americas | |
Processing methods | Back Pressure: 0.3 to 1.4MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |