Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Density of 1.19 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.09 % Show Supplier Material materials with Moisture absorption of 0.09 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.18 [-] Show Supplier Material materials with Relative density of 1.18 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.12 % Show Supplier Material materials with Water absorption of 0.12 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastic modulus of 2.1 GPa | ASTM D 638 | 50 mm/min |
Elongation | 23.0 °C | 4.8 % Show Supplier Material materials with Elongation of 4.8 % | ASTM D 638 | yld, Type I, 50 mm/min |
Flexural modulus | 23.0 °C | 2.1 GPa Show Supplier Material materials with Flexural modulus of 2.1 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Flexural strength | 23.0 °C | 86 MPa Show Supplier Material materials with Flexural strength of 86 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Impact strength, Izod notched | 23.0 °C | 810 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 810 kJ/m² | ASTM D 256 | notched, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 650 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 650 J/m | ASTM D 256 | notched, -30°C |
Tensile strength | 23.0 °C | 57 MPa Show Supplier Material materials with Tensile strength of 57 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Ball Pressure Test | pass | IEC 60695-10-2 | 125°C +/- 2°C | |
Heat deflection temperature | 116 °C Show Supplier Material materials with Heat deflection temperature of 116 °C | ||
Heat deflection temperature, 1.80 MPa | 116 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 116 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Vicat softening temperature | 138 °C Show Supplier Material materials with Vicat softening temperature of 138 °C | ISO 306 | Rate B/120 | |
Flammability | UL Recognized, 94HB Flame Class Rating: 0.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102217430- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 14 g/10min Show Supplier Material materials with Melt mass-flow rate of 14 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 13 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 13 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.4 % Show Supplier Material materials with Shrinkage, transverse of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover | |
Availability | Asia | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |