General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Density of 1.56 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.09 % Show Supplier Material materials with Moisture absorption of 0.09 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.56 [-] Show Supplier Material materials with Relative density of 1.56 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.23 % Show Supplier Material materials with Water absorption of 0.23 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 11 GPa Show Supplier Material materials with Elastic modulus of 11 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 175 MPa Show Supplier Material materials with Flexural strength of 175 MPa | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 72 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 72 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 37 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 570 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 570 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 108 MPa Show Supplier Material materials with Tensile strength of 108 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.2E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ||||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 125 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 125 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Vicat softening temperature | 220 °C Show Supplier Material materials with Vicat softening temperature of 220 °C | ISO 306 | Rate A/50 | |||
Flammability | UL Recognized, 94-5VB Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 750°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100522223- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 16 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 16 cm³/10min | ISO 1133 | MVR at 250°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.28 % Show Supplier Material materials with Shrinkage of 0.28 % | SABIC method | 3.2 mm |
Shrinkage, transverse | 23.0 °C | 0.57 % Show Supplier Material materials with Shrinkage, transverse of 0.57 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, EV Infrastructure, Data Transfer, Data Management, Inverter, Personal Computing, Power Manangement, Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 245 to 260.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |