General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Density of 1.31 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 31 % Show Supplier Material materials with Limiting oxygen index of 31 % | |
Moisture absorption | 23.0 °C | 0.08 % Show Supplier Material materials with Moisture absorption of 0.08 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.31 [-] Show Supplier Material materials with Relative density of 1.31 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastic modulus of 3.2 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ISO 527 | yield, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 70 MPa Show Supplier Material materials with Flexural strength of 70 MPa | ISO 178 | yield, 2 mm/min | ||
Impact strength, Charpy notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm | ||
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 40 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 40 J/m | ASTM D 256 | ||
Tensile strength | 23.0 °C | 38 MPa Show Supplier Material materials with Tensile strength of 38 MPa | ISO 527 | break, 50 mm/min | ||
Impact strength, Izod unnotched | ISO 180/1U | 80*10*4, 23°C | ||||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 0.8 mm | |||
Heat deflection temperature | 60 - 160 °C Show Supplier Material materials with Heat deflection temperature of 60 - 160 °C | ||||
Heat deflection temperature, 0.45 MPa | 160 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 60 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||
Vicat softening temperature | 170 °C Show Supplier Material materials with Vicat softening temperature of 170 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 700°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100208982- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 0 V Show Supplier Material materials with Comparative tracking index of 0 V | UL 746A | (UL) {PLC} |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 20 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 20 cm³/10min | ISO 1133 | MVR at 250°C/2.16 kg | |
Shrinkage | 23.0 °C | 1.8 % Show Supplier Material materials with Shrinkage of 1.8 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Facility Infrastructure, Electronic Components, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 230 to 240.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |