General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Density of 1.46 g/cm³ | ISO 1183 |
Relative density | 23.0 °C | 1.46 [-] Show Supplier Material materials with Relative density of 1.46 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 7.4 GPa Show Supplier Material materials with Elastic modulus of 7.4 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2 % Show Supplier Material materials with Elongation of 2 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 6.3 GPa Show Supplier Material materials with Flexural modulus of 6.3 GPa | ISO 178 | 2 mm/min |
Flexural strain | 23.0 °C | 3 % Show Supplier Material materials with Flexural strain of 3 % | ISO 178 | break, 2 mm/min |
Flexural strength | 23.0 °C | 125 MPa Show Supplier Material materials with Flexural strength of 125 MPa | ISO 178 | break, 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 142 MPa Show Supplier Material materials with Hardness, Ball Indentation of 142 MPa | ISO 2039-1 | H358/30 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ISO 2039-2 |
Impact strength, Charpy notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m² | ISO 179/2C | -30°C |
Impact strength, Charpy unnotched | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 20 kJ/m² | ISO 179/2C | -30°C |
Impact strength, Izod notched | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m² | ISO 180/1A | 80*10*4, 0°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 45 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 45 J/m | ASTM D 256 | notched, -30°C |
Impact strength, Izod unnotched | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 22 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 330 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 330 J/m | ASTM D 4812 | 23°C |
Tensile strength | 23.0 °C | 75 MPa Show Supplier Material materials with Tensile strength of 75 MPa | ISO 527 | yield, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 3.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 3.1E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 1.65E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.65E-4 1/K | ISO 11359-2 | 23°C to 150°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 0.8 mm | |||
Heat deflection temperature | 180 - 215 °C Show Supplier Material materials with Heat deflection temperature of 180 - 215 °C | ||||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 180 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 180 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Vicat softening temperature | 200 °C Show Supplier Material materials with Vicat softening temperature of 200 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 750°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 850°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 0.8 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100700420- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 1 V Show Supplier Material materials with Comparative tracking index of 1 V | UL 746A | (UL) {PLC} |
Dielectric constant, 1MHz | 23.0 °C | 3.3 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 3.3 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 38 kV/mm Show Supplier Material materials with Dielectric strength of 38 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 60250 |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 15 g/10min Show Supplier Material materials with Melt mass-flow rate of 15 g/10min | ISO 1133 | 250°C/5.0 kg | |
Melt viscosity | 23.0 °C | 145 Pa·s Show Supplier Material materials with Melt viscosity of 145 Pa·s | ISO 11443 | 260°C, 1500 sec-1 |
Melt volume-flow rate | 45 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 45 cm³/10min | ISO 1133 | MVR at 265°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |