General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 31 % Show Supplier Material materials with Limiting oxygen index of 31 % | |
Moisture absorption | 23.0 °C | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.45 [-] Show Supplier Material materials with Relative density of 1.45 [-] | ASTM D 792 | |
Water absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Water absorption of 0.15 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 7.5 GPa Show Supplier Material materials with Elastic modulus of 7.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 3 % Show Supplier Material materials with Elongation of 3 % | ISO 527 | break, 5 mm/min |
Flexural modulus | 23.0 °C | 6.4 GPa Show Supplier Material materials with Flexural modulus of 6.4 GPa | ISO 178 | 2 mm/min |
Flexural strain | 23.0 °C | 3 % Show Supplier Material materials with Flexural strain of 3 % | ISO 178 | break, 2 mm/min |
Flexural strength | 23.0 °C | 130 MPa Show Supplier Material materials with Flexural strength of 130 MPa | ISO 178 | break, 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 128 MPa Show Supplier Material materials with Hardness, Ball Indentation of 128 MPa | ISO 2039-1 | H358/30 |
Hardness, Rockwell R | 23.0 °C | 98 [-] Show Supplier Material materials with Hardness, Rockwell R of 98 [-] | ISO 2039-2 |
Impact strength, Charpy notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | ISO 179/2C | -30°C |
Impact strength, Charpy unnotched | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 25 kJ/m² | ISO 179/2C | -30°C |
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 | 0°C |
Impact strength, Izod unnotched | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 360 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 360 J/m | ASTM D 4812 | unnotched, -30°C |
Tensile strength | 23.0 °C | 80 MPa Show Supplier Material materials with Tensile strength of 80 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coefficient of thermal expansion | 23.0 °C | 4.2E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.2E-5 1/K | ISO 11359-2 | 23°C to 150°C |
Coefficient of thermal expansion, transverse | 23.0 °C | 1.73E-4 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 1.73E-4 1/K | ISO 11359-2 | 23°C to 150°C |
Heat deflection temperature | 200 - 220 °C Show Supplier Material materials with Heat deflection temperature of 200 - 220 °C | ||
Heat deflection temperature, 0.45 MPa | 220 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Vicat softening temperature | 205 °C Show Supplier Material materials with Vicat softening temperature of 205 °C | ISO 306 | Rate B/120 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1MHz | 23.0 °C | 3.7 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 3.7 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 28 kV/mm Show Supplier Material materials with Dielectric strength of 28 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Dissipation factor, 1MHz | 23.0 °C | 0.15 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.15 [-] | IEC 60250 |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 24 g/10min Show Supplier Material materials with Melt mass-flow rate of 24 g/10min | ASTM D 1238 | 265°C/5.0 kgf | |
Melt viscosity | 23.0 °C | 150 Pa·s Show Supplier Material materials with Melt viscosity of 150 Pa·s | ISO 11443 | 260°C, 1500 sec-1 |
Melt volume-flow rate | 18 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 18 cm³/10min | ISO 1133 | MVR at 265°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Coil bobbin, Electronic Components, Enclosures, Heavy Vehicles, Lab Ware and Clinical Diagnostics, EV Infrastructure, Displays, Wireless Communications, Personal Computing, Respiratory | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |