General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.35 % Show Supplier Material materials with Water absorption of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastic modulus of 2.3 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 6 % Show Supplier Material materials with Elongation of 6 % | ISO 527 | yield, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 96 MPa Show Supplier Material materials with Flexural strength of 96 MPa | ISO 178 | yield, 2 mm/min | ||
Impact strength, Charpy notched | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 65 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C | ||
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 130 J/m | ASTM D 256 | ||
Instrumented Impact, Total Energy | 23.0 °C | 80 J Show Supplier Material materials with Instrumented Impact, Total Energy of 80 J | ASTM D 3763 | 23°C | ||
Tensile strength | 23.0 °C | 67 MPa Show Supplier Material materials with Tensile strength of 67 MPa | ISO 527 | yield, 50 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | unnotched 80*10*3, 23°C, |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 124 °C Show Supplier Material materials with Heat deflection temperature of 124 °C | ||||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Vicat softening temperature | 140 °C Show Supplier Material materials with Vicat softening temperature of 140 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100462317- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index 960°C, passes at: 1.5mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1.5mm IEC 60695-2-12 <br> UV-light, water exposure/immersion: F2- UL 746C |
Optical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 17.5 g/10min Show Supplier Material materials with Melt mass-flow rate of 17.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 16 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 16 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Energy Management, Enclosure/Housing/Cover, Front Grille, Exterior Trim, Exterior, Lawn/Garden, Interior, Heavy Vehicles, Circuit Protection, Battery Pack, Antenna, All-Terrain Vehicle, Doors Hardware/Trim, Cowl Vent Grille, Displays, City, Wiring Devices, Spoiler, Non-LED Lighting, Oil/Gas, Personal Computing, LED Lighting, Meter Water, Power Boat, Recreational Vehicle, Plumbing, Smart/ID Card, Small Appliance | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |