General
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 23.0 °C | 130 % Show Supplier Material materials with Elongation of 130 % | ISO 527 | break, 50 mm/min |
Flexural modulus | 23.0 °C | 0.1 GPa Show Supplier Material materials with Flexural modulus of 0.1 GPa | ISO 178 | 12.5 mm/min |
Hardness, Shore A | 23.0 °C | 87 [-] Show Supplier Material materials with Hardness, Shore A of 87 [-] | ASTM D 2240 | 30S reading |
Tensile strength | 23.0 °C | 18 MPa Show Supplier Material materials with Tensile strength of 18 MPa | ISO 527 | break, 50 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | ASTM D 746 | |
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | IEC 60695-2-13 | 3.0 mm | |
Flammability | Smoke Density on 0.5mm plaque, Flame, Ds, max: 143- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 67- ASTM E 662 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | IEC 60112 | |
Dielectric constant, 1MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1MHz of 2.6 [-] | IEC 60250 |
Dielectric strength | 23.0 °C | 28 kV/mm Show Supplier Material materials with Dielectric strength of 28 kV/mm | IEC 60243-1 | in oil, 1.5mm |
Dissipation factor, 1MHz | 23.0 °C | 2.8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.8E-3 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 2.40E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.40E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 15 g/10min Show Supplier Material materials with Melt mass-flow rate of 15 g/10min | ASTM D 1238 | 250°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wire & cable | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |