Description

FLEX NORYL™ WCA871A resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 105C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCA871A resin is intended for evaluation in wire insulation and cable jacket applications in light colors. It has a Shore A Hardness reading of 84 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

28 %

Show Supplier Material materials with Limiting oxygen index of 28 %

Relative density

23.0 °C

1.06 [-]

Show Supplier Material materials with Relative density of 1.06 [-]

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

130 %

Show Supplier Material materials with Elongation of 130 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

0.1 GPa

Show Supplier Material materials with Flexural modulus of 0.1 GPa

ISO 178 | 12.5 mm/min

Hardness, Shore A

23.0 °C

87 [-]

Show Supplier Material materials with Hardness, Shore A of 87 [-]

ASTM D 2240 | 30S reading

Tensile strength

23.0 °C

18 MPa

Show Supplier Material materials with Tensile strength of 18 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyValueComment

Brittleness temperature

-40 °C

Show Supplier Material materials with Brittleness temperature of -40 °C

ASTM D 746

Glow Wire Ignition Temperature

825 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C

IEC 60695-2-13 | 3.0 mm

Flammability

Smoke Density on 0.5mm plaque, Flame, Ds, max: 143- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 67- ASTM E 662 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112 |

Dielectric constant, 1MHz

23.0 °C

2.6 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.6 [-]

IEC 60250

Dielectric strength

23.0 °C

28 kV/mm

Show Supplier Material materials with Dielectric strength of 28 kV/mm

IEC 60243-1 | in oil, 1.5mm

Dissipation factor, 1MHz

23.0 °C

2.8E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 2.8E-3 [-]

IEC 60250

Volume resistivity

23.0 °C

2.40E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.40E+16 Ω·cm

ASTM D 257

Rheological Properties

PropertyValueComment

Melt mass-flow rate

15 g/10min

Show Supplier Material materials with Melt mass-flow rate of 15 g/10min

ASTM D 1238 | 250°C/5.0 kgf

Technological properties

Property
Application areas

Wireless Communications, Wire & cable

Availability

Europe,Asia,Americas

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.