General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative density of 1.2 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastic modulus of 2.2 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 97 % Show Supplier Material materials with Elongation of 97 % | ISO 527 | break, 50 mm/min | ||
Flexural modulus | 23.0 °C | 2.2 GPa Show Supplier Material materials with Flexural modulus of 2.2 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 91 MPa Show Supplier Material materials with Flexural strength of 91 MPa | ISO 178 | yield, 2 mm/min | ||
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D 785 | ||
Impact strength, Charpy notched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Impact strength, Izod notched | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 115 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 115 J/m | ASTM D 256 | notched, -30°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 56 J Show Supplier Material materials with Instrumented Impact, Total Energy of 56 J | ASTM D 3763 | 23°C | ||
Tensile strength | 23.0 °C | 56 MPa Show Supplier Material materials with Tensile strength of 56 MPa | ISO 527 | break, 50 mm/min | ||
Impact strength, Charpy unnotched | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Impact strength, Izod unnotched | ISO 180/1U | unnotched 80*10*3, -30°C |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | PASS | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature | 115 - 121 °C Show Supplier Material materials with Heat deflection temperature of 115 - 121 °C | ||||
Heat deflection temperature, 0.45 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 121 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat softening temperature | 130 °C Show Supplier Material materials with Vicat softening temperature of 130 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100910216- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥0.5mm UL 94 |
Optical
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 40 g/10min Show Supplier Material materials with Melt mass-flow rate of 40 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 38 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 38 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, LED Lighting, Monitoring and Imaging, Meter Water, Safety Glasses, Seating/Chair, Small Appliance, Surgical Devices, Wireless Communications, Wiring Devices, Wearables, Vacuum Cleaner, Cooking Range, Audio, Electronic Components, Enclosure/Housing/Cover, Energy Management, Enclosures, Individual Equiptment, Infotainment/Telematic, Interior, Freezer | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 105 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |