General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Density of 1.25 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.27 [-] Show Supplier Material materials with Relative density of 1.27 [-] | ASTM D 792 |
Water absorption | 23.0 °C | 0.25 % Show Supplier Material materials with Water absorption of 0.25 % | ISO 62-1 | (23°C/saturated) |
Mechanical
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elastic modulus | 23.0 °C | 3.4 GPa Show Supplier Material materials with Elastic modulus of 3.4 GPa | ISO 527 | 1 mm/min | ||
Elongation | 23.0 °C | 7 % Show Supplier Material materials with Elongation of 7 % | ISO 527 | break, 5 mm/min | ||
Flexural modulus | 23.0 °C | 3.3 GPa Show Supplier Material materials with Flexural modulus of 3.3 GPa | ISO 178 | 2 mm/min | ||
Flexural strength | 23.0 °C | 97 MPa Show Supplier Material materials with Flexural strength of 97 MPa | ISO 178 | yield, 2 mm/min | ||
Impact strength, Charpy notched | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C | ||
Impact strength, Charpy unnotched | 23.0 °C | 75 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m² | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||
Impact strength, Izod notched | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 65 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 65 J/m | ASTM D 256 | notched, -30°C | ||
Impact strength, Izod unnotched | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 65 kJ/m² | ISO 180/1U | 80*10*3, 23°C | ||
Tensile strength | 23.0 °C | 58 MPa Show Supplier Material materials with Tensile strength of 58 MPa | ISO 527 | yield, 5 mm/min | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | unnotched, -30°C |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | passes | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coefficient of thermal expansion | 23.0 °C | 4.1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 4.1E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.4E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.4E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Flammability Index | 930 °C Show Supplier Material materials with Glow Wire Flammability Index of 930 °C | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature | 142 °C Show Supplier Material materials with Heat deflection temperature of 142 °C | ||||
Heat deflection temperature, 1.80 MPa | 142 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 142 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | UL 746B | |||
Vicat softening temperature | 155 °C Show Supplier Material materials with Vicat softening temperature of 155 °C | ISO 306 | Rate B/120 | |||
Flammability | Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102888979- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 3 V Show Supplier Material materials with Comparative tracking index of 3 V | UL 746A | (UL) {PLC} |
Dielectric strength | 23.0 °C | 32 kV/mm Show Supplier Material materials with Dielectric strength of 32 kV/mm | IEC 60243-1 | in oil, 1.5mm |
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt mass-flow rate | 11 g/10min Show Supplier Material materials with Melt mass-flow rate of 11 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Melt volume-flow rate | 27 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 27 cm³/10min | ISO 1133 | MVR at 330°C/1.2 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Availability | Europe | |
Processing methods | Rear - Zone 1 Temperature: 290 to 310.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |