ULTEM™ Resin 3452 - Asia

Want to keep this datasheet? Save it now in your required format

Description

45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.

This material data has been provided by Sabic.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.4 %

Show Supplier Material materials with Elongation of 1.4 %

ASTM D 638 | brk, Type I, 5 mm/min

Flexural modulus

23.0 °C

12.4 GPa

Show Supplier Material materials with Flexural modulus of 12.4 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

179 MPa

Show Supplier Material materials with Flexural strength of 179 MPa

ASTM D 790 | brk, 2.6 mm/min, 100 mm span

Impact strength, Izod notched

23.0 °C

58 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 58 kJ/m²

ASTM D 256 | notched, 23°C

Tensile strength

23.0 °C

131 MPa

Show Supplier Material materials with Tensile strength of 131 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

212 °C

Show Supplier Material materials with Heat deflection temperature of 212 °C

Heat deflection temperature, 1.80 MPa

212 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

180 °C

Show Supplier Material materials with Relative temperature index, electrical of 180 °C

UL 746B

Relative temperature index, mechanical impact

180 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 180 °C

UL 746B

Relative temperature index, mechanical strength

180 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C

UL 746B

Flammability

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221107- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.77mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

4 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.25 %

Show Supplier Material materials with Shrinkage of 0.25 %

SABIC method | on tensile bar

Technological properties

Property
Application areas

Electronic Components, Gear/Bearing/Slider, Data Transfer, Auto Aftermarket, Aerospace, Wireless Communications, Underhood

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 150°C
Drying Time: 4 to 6.0hrs
Drying Time (Cumulative): 24hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 350 to 400.0°C
Nozzle Temperature: 345 to 400.0°C
Front - Zone 3 Temperature: 345 to 400.0°C
Middle - Zone 2 Temperature: 340 to 400.0°C
Rear - Zone 1 Temperature: 330 to 400.0°C
Mold Temperature: 135 to 165.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 40 to 70.0rpm
Shot to Cylinder Size: 40 to 60.0%
Vent Depth: 0.025 to 0.076mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.