General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Density of 1.37 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 8.5 GPa Show Supplier Material materials with Elastic modulus of 8.5 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.9 % Show Supplier Material materials with Elongation of 2.9 % | ISO 527 | break |
Flexural modulus | 23.0 °C | 8.1 GPa Show Supplier Material materials with Flexural modulus of 8.1 GPa | ISO 178 |
Flexural strength | 23.0 °C | 203 MPa Show Supplier Material materials with Flexural strength of 203 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Tensile strength | 23.0 °C | 160 MPa Show Supplier Material materials with Tensile strength of 160 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Flammability | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101281583- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Comparative tracking index | 23.0 °C | 375 V Show Supplier Material materials with Comparative tracking index of 375 V | IEC 60112 | M |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Displays, Data Management, Electronic Components, Enclosure/Housing/Cover, Rail Cabin Interiors, Photo/Video Camera, Oil/Gas, Personal Care, Medical Device, Medical Facility Infrastructure, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 80 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |