General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.1 g/cm³ Show Supplier Material materials with Density of 1.1 g/cm³ | ISO 1183 |
Limiting oxygen index | 23.0 °C | 21 % Show Supplier Material materials with Limiting oxygen index of 21 % | |
Relative density | 23.0 °C | 1.14 [-] Show Supplier Material materials with Relative density of 1.14 [-] | ASTM D 792 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastic modulus of 2.3 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 4 % Show Supplier Material materials with Elongation of 4 % | ISO 527 | yield, 50 mm/min |
Flexural modulus | 23.0 °C | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 80 MPa Show Supplier Material materials with Flexural strength of 80 MPa | ISO 178 | yield, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Impact strength, Izod notched | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Tensile strength | 23.0 °C | 50 MPa Show Supplier Material materials with Tensile strength of 50 MPa | ISO 527 | yield, 50 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 8.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 8.7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature | 95 - 114 °C Show Supplier Material materials with Heat deflection temperature of 95 - 114 °C | ||||
Heat deflection temperature, 0.45 MPa | 114 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 114 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Vicat softening temperature | 115 °C Show Supplier Material materials with Vicat softening temperature of 115 °C | ISO 306 | Rate B/120 | |||
Flammability | UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344461- - |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt volume-flow rate | 26 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 26 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg | |
Shrinkage | 23.0 °C | 0.5 % Show Supplier Material materials with Shrinkage of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Doors Hardware/Trim, Data Transfer, Data Management, Enclosures, Pharmaceutical Packaging & Drug Delivery, Personal Computing, Wireless Communications | |
Availability | Europe,Americas | |
Processing methods | Hopper Temperature: 60 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |