ULTEM™ Resin HU1110 - Europe

Want to keep this datasheet? Save it now in your required format

Description

Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change; biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.36 g/cm³

Show Supplier Material materials with Density of 1.36 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.65 %

Show Supplier Material materials with Moisture absorption of 0.65 %

ISO 62 | (23°C / 50% RH)

Water absorption

23.0 °C

1.2 %

Show Supplier Material materials with Water absorption of 1.2 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.5 GPa

Show Supplier Material materials with Elastic modulus of 3.5 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

6 %

Show Supplier Material materials with Elongation of 6 %

ISO 527 | yield, 5 mm/min

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

140 MPa

Show Supplier Material materials with Flexural strength of 140 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 4 kJ/m²

ISO 180/1A | notched 80*10*4, -30°C

Tensile strength

23.0 °C

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

ISO 527 | yield, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Vicat softening temperature

200 °C

Show Supplier Material materials with Vicat softening temperature of 200 °C

ISO 306 | Rate B/50

Flammability

UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100044748- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 3

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm

≥, UL 746A | PLC 2

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

21 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 21 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Monitoring and Imaging, Respiratory, Electronic Components

Availability

Europe,Asia,Americas

Features

High Stiffness, Healthcare management of change, Steam, Gamma, EtO and E-beam sterilizable, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Steam Sterilizable, Gamma Sterilizable, E-beam Sterilizable, Food Contact Acceptable, Biocompatible

Processing methods

Melt Temperature: 350 to 400.0°C
Shot to Cylinder Size: 40 to 60.0%
Drying Time (Cumulative): 24hrs
Mold Temperature: 135 to 165.0°C
Vent Depth: 0.025 to 0.076mm
Front - Zone 3 Temperature: 345 to 400.0°C
Nozzle Temperature: 345 to 400.0°C
Middle - Zone 2 Temperature: 340 to 400.0°C
Back Pressure: 0.3 to 0.7MPa
Rear - Zone 1 Temperature: 330 to 400.0°C
Drying Temperature: 150°C
Drying Time: 4 to 6.0hrs
Screw Speed: 40 to 70.0rpm
Maximum Moisture Content: 0.02%

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.