All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Density of 1.27 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

47 %

Show Supplier Material materials with Limiting oxygen index of 47 %

Moisture absorption

23.0 °C

0.7 %

Show Supplier Material materials with Moisture absorption of 0.7 %

ISO 62 | (23°C / 50% RH)

Water absorption

23.0 °C

1.25 %

Show Supplier Material materials with Water absorption of 1.25 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.2 GPa

Show Supplier Material materials with Elastic modulus of 3.2 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

60 %

Show Supplier Material materials with Elongation of 60 %

ISO 527 | break, 5 mm/min

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

160 MPa

Show Supplier Material materials with Flexural strength of 160 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Izod notched

23.0 °C

5 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 5 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Taber Abrasion

23.0 °C

10 mg/1000cy

Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy

SABIC method | CS-17, 1 kg

Tensile strength

23.0 °C

105 MPa

Show Supplier Material materials with Tensile strength of 105 MPa

ISO 527 | yield, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

193 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 193 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Vicat softening temperature

211 °C

Show Supplier Material materials with Vicat softening temperature of 211 °C

ISO 306 | Rate B/50

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100044748- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

Dielectric strength

23.0 °C

25 kV/mm

Show Supplier Material materials with Dielectric strength of 25 kV/mm

IEC 60243-1 | in oil, 1.6 mm

Dissipation factor

23.0 °C

2.5E-3 [-]

Show Supplier Material materials with Dissipation factor of 2.5E-3 [-]

IEC 60250 | 2450 MHz

High Amp Arc Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm

IEC 60093 |

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

13 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 13 cm³/10min

ISO 1133 | MVR at 340°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | on tensile bar

Technological properties

Property
Application areas

Medical Facility Infrastructure, Meter Gas, Monitoring and Imaging, Medical Device, Pharmaceutical Packaging & Drug Delivery, Renal and Blood Handling, Respiratory, Surgical Devices, Lab Ware and Clinical Diagnostics, Lawn/Garden, Fused Deposition Modeling (FDM), Fluid Delivery, Enclosures, Electronic Components, Wire & cable

Availability

Europe,Asia,Americas

Features

High Stiffness, Healthcare management of change, Steam, Gamma, EtO and E-beam sterilizable, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Steam Sterilizable, Gamma Sterilizable, E-beam Sterilizable, Food Contact Acceptable, Biocompatible

Processing methods

Drying Temperature: 150°C
Drying Time: 4 to 6.0hrs
Rear - Zone 1 Temperature: 340 to 395.0°C
Nozzle Temperature: 350 to 405.0°C
Middle - Zone 2 Temperature: 350 to 405.0°C
Melt Temperature: 370 to 410.0°C
Hopper Temperature: 80 to 120.0°C
Maximum Moisture Content: 0.02%
Front - Zone 3 Temperature: 360 to 415.0°C
Mold Temperature: 140 to 180.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.