Description

PTFE filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL 94 V0 and 5VA listing in recognized colors.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.33 g/cm³

Show Supplier Material materials with Density of 1.33 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.6 %

Show Supplier Material materials with Moisture absorption of 0.6 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.33 [-]

Show Supplier Material materials with Relative density of 1.33 [-]

ASTM D 792

Water absorption

23.0 °C

1.1 %

Show Supplier Material materials with Water absorption of 1.1 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Elastic modulus of 3.3 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

3.1 GPa

Show Supplier Material materials with Flexural modulus of 3.1 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

130 MPa

Show Supplier Material materials with Flexural strength of 130 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A | notched 80*10*4, -30°C

Impact strength, Izod notched, ASTM

23.0 °C

117 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

380 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 380 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

100 MPa

Show Supplier Material materials with Tensile strength of 100 MPa

ISO 527 | yield, 50 mm/min

Thermal

PropertyTemperatureValueComment

Ball Pressure Test

Passes

IEC 60695-10-2 | 125°C +/- 2°C

Coefficient of thermal expansion

23.0 °C

3.9E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3.9E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

23.0 °C

4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 4E-5 1/K

ISO 11359-2 | 23°C to 150°C

Heat deflection temperature, 1.80 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Vicat softening temperature

215 °C

Show Supplier Material materials with Vicat softening temperature of 215 °C

ISO 306 | Rate B/50

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.38mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.9mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221111- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 3

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

9.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 9.5 g/10min

ASTM D 1238 | 337°C/6.6 kgf

Melt volume-flow rate

13 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 13 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Shrinkage

23.0 °C

0.6 %

Show Supplier Material materials with Shrinkage of 0.6 %

SABIC method | on tensile bar

Shrinkage, transverse

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage, transverse of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Enclosures, Cooking Range, Oil/Gas

Availability

Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Wear resistant

Processing methods

Back Pressure: 0.3 to 0.7MPa
Vent Depth: 0.025 to 0.076mm
Drying Time: 4 to 6.0hrs
Front - Zone 3 Temperature: 350 to 370.0°C
Middle - Zone 2 Temperature: 345 to 365.0°C
Rear - Zone 1 Temperature: 340 to 360.0°C
Shot to Cylinder Size: 40 to 60.0%
Melt Temperature: 350 to 370.0°C
Drying Time (Cumulative): 10hrs
Maximum Moisture Content: 0.02%
Screw Speed: 40 to 70.0rpm
Drying Temperature: 135°C
Nozzle Temperature: 350 to 370.0°C
Mold Temperature: 135 to 165.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.