20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

50 %

Show Supplier Material materials with Limiting oxygen index of 50 %

Water absorption

23.0 °C

0.19 %

Show Supplier Material materials with Water absorption of 0.19 %

ASTM D 570 | (23°C/24hrs)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

6.89 GPa

Show Supplier Material materials with Elastic modulus of 6.89 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

4 %

Show Supplier Material materials with Elongation of 4 %

ASTM D 638 | brk, Type I, 5 mm/min

Flexural modulus

23.0 °C

6.89 GPa

Show Supplier Material materials with Flexural modulus of 6.89 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

227 MPa

Show Supplier Material materials with Flexural strength of 227 MPa

ASTM D 790 | brk, 2.6 mm/min, 100 mm span

Tensile strength

23.0 °C

131 MPa

Show Supplier Material materials with Tensile strength of 131 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.52E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.52E-5 1/K

ASTM E 831 | -20°C to 150°C

Heat deflection temperature

210 °C

Show Supplier Material materials with Heat deflection temperature of 210 °C

Heat deflection temperature, 0.45 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 210 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Vicat softening temperature

220 °C

Show Supplier Material materials with Vicat softening temperature of 220 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94-5VA Flame Class Rating: ≥1.9mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.41mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 1.3- ASTM E 662 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221093- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=502535- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

Dielectric strength

23.0 °C

26.3 kV/mm

Show Supplier Material materials with Dielectric strength of 26.3 kV/mm

ASTM D 149 | in oil, 1.6 mm

Dissipation factor

23.0 °C

4.9E-3 [-]

Show Supplier Material materials with Dissipation factor of 4.9E-3 [-]

ASTM D 150 | 2450 MHz

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm

≥, UL 746A | PLC 2

Volume resistivity

23.0 °C

7.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 7.00E+16 Ω·cm

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Meter Water, Medical Device, Oil/Gas, Non-LED Lighting, Personal Computing, Pharmaceutical Packaging & Drug Delivery, Power Manangement, Wireless Communications, Weapon, Water Treatment/Filtration, Wiring Devices, Data Transfer, Displays, Circuit Protection, Aircraft Seating, Aerospace, Air Cabin Interiors, Fluid Delivery, Individual Equiptment, Enclosures, Enclosure/Housing/Cover, Electronics, Electronic Components, Wire & cable

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, General Purpose, High Heat Resistance, Good dimensional stability, Flame Retardant

Processing methods

Drying Temperature: 150°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 40 to 70.0rpm
Front - Zone 3 Temperature: 345 to 400.0°C
Drying Time (Cumulative): 24hrs
Middle - Zone 2 Temperature: 340 to 400.0°C
Melt Temperature: 350 to 400.0°C
Drying Time: 4 to 6.0hrs
Mold Temperature: 135 to 165.0°C
Nozzle Temperature: 345 to 400.0°C
Rear - Zone 1 Temperature: 330 to 400.0°C
Vent Depth: 0.025 to 0.076mm
Maximum Moisture Content: 0.02%
Shot to Cylinder Size: 40 to 60.0%

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.