Description

10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

4.61 GPa

Show Supplier Material materials with Elastic modulus of 4.61 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

6 %

Show Supplier Material materials with Elongation of 6 %

ASTM D 638 | brk, Type I, 5 mm/min

Flexural modulus

23.0 °C

5.24 GPa

Show Supplier Material materials with Flexural modulus of 5.24 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

199 MPa

Show Supplier Material materials with Flexural strength of 199 MPa

ASTM D 790 | brk, 2.6 mm/min, 100 mm span

Tensile strength

23.0 °C

114 MPa

Show Supplier Material materials with Tensile strength of 114 MPa

ASTM D 638 | yld, Type I, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

207 °C

Show Supplier Material materials with Heat deflection temperature of 207 °C

Heat deflection temperature, 1.80 MPa

207 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 207 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.41mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.9mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=502535- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100732301- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 4

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Technological properties

Property
Application areas

Personal Computing, Personal Care, Wireless Communications, Data Transfer, Data Management, Displays, Aircraft Seating, Building Accessory, Electronic Components, Enclosures

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, Easy Flow, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, General Purpose, High Heat Resistance, Good dimensional stability, Flame Retardant, Good Mold Release

Processing methods

Mold Temperature: 135 to 165.0°C
Melt Temperature: 350 to 400.0°C
Screw Speed: 40 to 70.0rpm
Back Pressure: 0.3 to 0.7MPa
Middle - Zone 2 Temperature: 340 to 400.0°C
Vent Depth: 0.025 to 0.076mm
Maximum Moisture Content: 0.02%
Drying Time: 4 to 6.0hrs
Drying Temperature: 150°C
Drying Time (Cumulative): 24hrs
Nozzle Temperature: 345 to 400.0°C
Front - Zone 3 Temperature: 345 to 400.0°C
Shot to Cylinder Size: 40 to 60.0%
Rear - Zone 1 Temperature: 330 to 400.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.