Enhanced flow Polyetherimide (Tg 217C). ECO Conforming.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.5 GPa

Show Supplier Material materials with Elastic modulus of 3.5 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

10 %

Show Supplier Material materials with Elongation of 10 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

140 MPa

Show Supplier Material materials with Flexural strength of 140 MPa

ISO 178 | yield, 2 mm/min

Tensile strength

23.0 °C

80 MPa

Show Supplier Material materials with Tensile strength of 80 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

185 °C

Show Supplier Material materials with Heat deflection temperature of 185 °C

Heat deflection temperature, 1.80 MPa

185 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 185 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101048292- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 3

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm

≥, UL 746A | PLC 2

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Surgical Devices, Air Cabin Interiors

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, High Pigment Load, Easy Flow, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, General Purpose, High Heat Resistance, Good dimensional stability, Flame Retardant

Processing methods

Front - Zone 3 Temperature: 370 to 410.0°C
Drying Temperature: 150°C
Nozzle Temperature: 360 to 400.0°C
Drying Time: 4 to 6.0hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 360 to 400.0°C
Middle - Zone 2 Temperature: 360 to 400.0°C
Rear - Zone 1 Temperature: 340 to 380.0°C
Mold Temperature: 140 to 180.0°C
Hopper Temperature: 80 to 100.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.