ULTEMTM 1000F resin is an amorphous, transparent polyetherimide (PEI) plastic offering a glass transition temperature (Tg) of 217?C. This inherently flame retardant resin has UL94 V0, V2 and 5VA ratings and is RoHS, US FDA and EU Food Contact compliant, with NSF 51 listing. ULTEMTM 1000F resin is an unreinforced general purpose grade offering high heat resistance, high strength and modulus and broad chemical resistance up to high temperatures.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

47 %

Show Supplier Material materials with Limiting oxygen index of 47 %

Water absorption

23.0 °C

1.25 %

Show Supplier Material materials with Water absorption of 1.25 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.2 GPa

Show Supplier Material materials with Elastic modulus of 3.2 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

6 %

Show Supplier Material materials with Elongation of 6 %

ISO 527 | yield, 50 mm/min

Flexural modulus

23.0 °C

3.3 GPa

Show Supplier Material materials with Flexural modulus of 3.3 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

160 MPa

Show Supplier Material materials with Flexural strength of 160 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Izod notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180/1A | 80*10*4, -30°C

Taber Abrasion

23.0 °C

10 mg/1000cy

Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy

SABIC method | CS-17, 1 kg

Tensile strength

23.0 °C

85 MPa

Show Supplier Material materials with Tensile strength of 85 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Heat deflection temperature

190 - 200 °C

Show Supplier Material materials with Heat deflection temperature of 190 - 200 °C

Heat deflection temperature, 0.45 MPa

200 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

ISO 75/Be | Edgew 120*10*4 sp=100mm

Heat deflection temperature, 1.80 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

170 °C

Show Supplier Material materials with Relative temperature index, electrical of 170 °C

UL 746B

Relative temperature index, mechanical impact

170 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C

UL 746B

Relative temperature index, mechanical strength

170 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C

UL 746B

Thermal conductivity

23.0 °C

0.24 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.24 W/(m·K)

ISO 8302

Vicat softening temperature

215 °C

Show Supplier Material materials with Vicat softening temperature of 215 °C

ISO 306 | Rate A/50

Flammability

Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101048254- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

Dielectric strength

23.0 °C

33 kV/mm

Show Supplier Material materials with Dielectric strength of 33 kV/mm

IEC 60243-1 | in oil, 0.8 mm

Dissipation factor

23.0 °C

2.5E-3 [-]

Show Supplier Material materials with Dissipation factor of 2.5E-3 [-]

IEC 60250 | 2450 MHz

High Amp Arc Ignition

23.0 °C

3 mm

Show Supplier Material materials with High Amp Arc Ignition of 3 mm

≥, UL 746A | PLC 3

High Volt Arc Track Rate

23.0 °C

2 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm

≥, UL 746A | PLC 2

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm

IEC 60093 |

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Wireless Communications, Tray, Surgical Tray, Oil/Gas, Personal Care, Medical Device, Laundry Dryer, Monitoring and Imaging, Power Manangement, Refrigerator, Surgical Devices, Semiconductor, Respiratory, Commercial Storage/Cookware, Coffee Maker/Espresso Machine, Data Management, Displays, Airline Service, Building Accessory, Aerospace, Aircraft Seating, Air Cabin Interiors, Electronic Components, Enclosure/Housing/Cover, Electronic Material Handling, Food Processor

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, General Purpose, High Heat Resistance, Good dimensional stability, Flame Retardant, Food Contact Acceptable

Processing methods

Drying Time: 4 to 6.0hrs
Front - Zone 3 Temperature: 360 to 415.0°C
Middle - Zone 2 Temperature: 350 to 405.0°C
Rear - Zone 1 Temperature: 340 to 395.0°C
Drying Temperature: 150°C
Maximum Moisture Content: 0.02%
Mold Temperature: 140 to 180.0°C
Melt Temperature: 370 to 410.0°C
Hopper Temperature: 80 to 120.0°C
Nozzle Temperature: 350 to 405.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.