FLEX NORYL™ WCD801A resin is a flexible, non-reinforced, migration improved, extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 80C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCD801A resin is intended for evaluation in wire insulation and cable jacket applications in dark colors. It has a Shore A Hardness reading of 80 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

26 %

Show Supplier Material materials with Limiting oxygen index of 26 %

Relative density

23.0 °C

1.1 [-]

Show Supplier Material materials with Relative density of 1.1 [-]

ASTM D 792 |

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

119 %

Show Supplier Material materials with Elongation of 119 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

0.09 GPa

Show Supplier Material materials with Flexural modulus of 0.09 GPa

ISO 178 | 12.5 mm/min

Hardness, Shore A

23.0 °C

80 [-]

Show Supplier Material materials with Hardness, Shore A of 80 [-]

ASTM D 2240 | 30S reading

Tensile strength

23.0 °C

13 MPa

Show Supplier Material materials with Tensile strength of 13 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyValueComment

Brittleness temperature

-40 °C

Show Supplier Material materials with Brittleness temperature of -40 °C

<, ASTM D 746

Flammability

Smoke Density on 0.5mm plaque, Flame, Ds, max: 142- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 95- ASTM E 662 <br> Glow Wire Flammability Index 650°C, passes at: 3mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=536311- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112 |

Dielectric constant, 1MHz

23.0 °C

2.8 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.8 [-]

IEC 60250

Dielectric constant, 60Hz

23.0 °C

2.8 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-]

IEC 60250 | 50/60 Hz

Dielectric strength

23.0 °C

23 kV/mm

Show Supplier Material materials with Dielectric strength of 23 kV/mm

IEC 60243-1 | in oil, 2.0mm

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

IEC 60250

Dissipation factor, 50Hz

23.0 °C

0.03 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 0.03 [-]

IEC 60250 | 50/60 Hz

Volume resistivity

23.0 °C

3.80E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 3.80E+15 Ω·cm

IEC 60093 |

Rheological Properties

PropertyValueComment

Melt mass-flow rate

11 g/10min

Show Supplier Material materials with Melt mass-flow rate of 11 g/10min

ASTM D 1238 | 250°C/5.0 kgf

Technological properties

Property
Application areas

Wireless Communications, Personal Computing, Enclosure/Housing/Cover, Heavy Vehicles, Freezer, Wire & cable

Availability

Americas

Features

Flexible, Hydrolytic Stability, Low Creep Sensitivity, Flame Retardant, Thin Wall, Non-Halogenated, Non-Chlorinated, Non-Brominated, Good Processability, Ductile

Processing methods

Melt Temperature: 220 to 250.0°C
Neck Temperature: 220 to 250.0°C
Head Zone Temperature: 220 to 250.0°C
Die Temperature: 220 to 250.0°C
Screw Speed: 15 to 85.0rpm
Screen Pack: 150 to 100.0-
Cross-head Temperature: 220 to 250.0°C
Water Bath Temperature: 15 to 60.0°C
Drying Time: 5 to 7.0hrs
Feed Zone Temperature: 180 to 220.0°C
Conductor Pre-heat Temperature: 25 to 120.0°C
Maximum Moisture Content: 0.02%
Drying Time (Cumulative): 12hrs
Middle Zone Temperatures: 220 to 250.0°C
Cooling Water Air Gap: 100 to 200.0mm
Drying Temperature: 75 to 85.0°C
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1-

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.