FLEX NORYL™ Resin WCA901 - Asia

Want to keep this datasheet? Save it now in your required format

Description

FLEX NORYL™ WCA901 resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 105C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCA901 resin is intended for evaluation in wire and cable applications. It has a Shore A Hardness reading of 91 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

27 %

Show Supplier Material materials with Limiting oxygen index of 27 %

Relative density

23.0 °C

1.1 [-]

Show Supplier Material materials with Relative density of 1.1 [-]

ASTM D 792 |

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

95 %

Show Supplier Material materials with Elongation of 95 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

0.39 GPa

Show Supplier Material materials with Flexural modulus of 0.39 GPa

ISO 178 | 12.5 mm/min

Hardness, Shore A

23.0 °C

91 [-]

Show Supplier Material materials with Hardness, Shore A of 91 [-]

ASTM D 2240 | 30S reading

Tensile strength

23.0 °C

22 MPa

Show Supplier Material materials with Tensile strength of 22 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyValueComment

Brittleness temperature

-40 °C

Show Supplier Material materials with Brittleness temperature of -40 °C

<, ASTM D 746

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112 |

Dielectric constant, 1MHz

23.0 °C

2.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

IEC 60250

Sheet resistivity, ROA

23.0 °C

4.20E+16 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 4.20E+16 Ω

ASTM D 257

Volume resistivity

23.0 °C

5.10E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 5.10E+15 Ω·cm

ASTM D 257

Rheological Properties

PropertyValueComment

Melt mass-flow rate

10 g/10min

Show Supplier Material materials with Melt mass-flow rate of 10 g/10min

ASTM D 1238 | 250°C/10.0 kgf

Technological properties

Property
Application areas

Wire & cable

Availability

Europe,Americas

Features

Flexible, Hydrolytic Stability, Low Creep Sensitivity, Flame Retardant, Thin Wall, Non-Halogenated, Non-Chlorinated, Non-Brominated, Good Processability, Ductile

Processing methods

Middle Zone Temperatures: 240 to 270.0°C
Die Temperature: 240 to 270.0°C
Conductor Pre-heat Temperature: 80 to 150.0°C
Cooling Water Air Gap: 100 to 200.0mm
Feed Zone Temperature: 200 to 240.0°C
Melt Temperature: 240 to 270.0°C
Screw Speed: 15 to 85.0rpm
Maximum Moisture Content: 0.02%
Drying Time: 5 to 7.0hrs
Cross-head Temperature: 240 to 270.0°C
Water Bath Temperature: 15 to 45.0°C
Head Zone Temperature: 240 to 270.0°C
Screen Pack: 150 to 100.0-
Drying Time (Cumulative): 12hrs
Neck Temperature: 240 to 270.0°C
Drying Temperature: 75 to 85.0°C
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1-

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.