Description

NORYL™ 731 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits good surface appearance, high ductility, and good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL 731 resin is an excellent candidate for a variety of applications.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Moisture absorption

23.0 °C

0.04 %

Show Supplier Material materials with Moisture absorption of 0.04 %

ISO 62-4 | (23°C/50% RH/Equilibrium)

Water absorption

23.0 °C

0.23 %

Show Supplier Material materials with Water absorption of 0.23 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Elastic modulus of 2.3 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

17 %

Show Supplier Material materials with Elongation of 17 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

2.2 GPa

Show Supplier Material materials with Flexural modulus of 2.2 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

80 MPa

Show Supplier Material materials with Flexural strength of 80 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm

Impact strength, Izod notched

23.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Tensile strength

23.0 °C

40 MPa

Show Supplier Material materials with Tensile strength of 40 MPa

ISO 527 | yield, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9.18E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.18E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

7E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7E-5 1/K

ISO 11359-2 | 23°C to 80°C

Heat deflection temperature, 1.80 MPa

120 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

105 °C

Show Supplier Material materials with Relative temperature index, electrical of 105 °C

UL 746B

Relative temperature index, mechanical impact

90 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C

UL 746B

Relative temperature index, mechanical strength

105 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B

Vicat softening temperature

143 °C

Show Supplier Material materials with Vicat softening temperature of 143 °C

ISO 306 | Rate B/120

Flammability

Glow Wire Flammability Index 750°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236745- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

2 V

Show Supplier Material materials with Comparative tracking index of 2 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 3

High Volt Arc Track Rate

23.0 °C

4 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

6 mm

Show Supplier Material materials with Hot-Wire Ignition of 6 mm

≥, UL 746A | PLC 4

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

9 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 9 cm³/10min

ISO 1133 | MVR at 280°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | on tensile bar

Technological properties

Property
Application areas

Meter Gas, Ignition System, Monitoring and Imaging, Meter Water, Laundry Dryer, LED Lighting, Medical Device, Personal Computing, Non-LED Lighting, Sanitary, Small Appliance, Security/Detection, Renal and Blood Handling, Refrigerator, Recreational Vehicle, Power Boat, Pipe/Fitting, Pump, Plumbing, Pharmaceutical Packaging & Drug Delivery, Wireless Communications, Wiring Devices, Watch/Jewelry, Water Treatment/Filtration, Wheel Cover, Wearables, Swimming Pool/Spa, Surgical Tray, Vending Machine, Washing Machine, Auto Electrical, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, ATM/Ticket Machine, Amusement Machine, Animal Testing, Aerospace, Coffee Maker/Espresso Machine, Bottles, Building Element, Building/Construction Sheet, Data Management, Doors Hardware/Trim, Conveyor, Dishwasher, Displays, Document Handling, EV Infrastructure, Food Transportation, Furnace/Heater, Fixture Bath/Shower, Lawn/Garden, Lab Ware and Clinical Diagnostics, Heavy Vehicles, Gas/Electric Oven, Hot Water System, Head Protection, Electronic Components, Enclosure/Housing/Cover, Electronics, Enclosures

Availability

Americas

Features

Hydrolytic Stability, Low Creep Sensitivity

Processing methods

Barrel - Zone 3 Temperature: 250 to 270.0°C
Drying Time: 2 to 3.0hrs
Drying Temperature: 100 to 120.0°C
Calibrator Temperature: 60 to 80.0°C
Barrel - Zone 4 Temperature: 250 to 270.0°C
Hopper Temperature: 60 to 80.0°C
Rear - Zone 1 Temperature: 240 to 260.0°C
Melt Temperature: 250 to 270.0°C
Hopper Temperature: 40 to 60.0°C
Barrel - Zone 2 Temperature: 230 to 250.0°C
Middle - Zone 2 Temperature: 260 to 280.0°C
Melt Temperature: 280 to 300.0°C
Barrel - Zone 1 Temperature: 220 to 240.0°C
Drying Time: 2 to 3.0hrs
Adapter Temperature: 250 to 270.0°C
Front - Zone 3 Temperature: 280 to 300.0°C
Nozzle Temperature: 260 to 280.0°C
Mold Temperature: 80 to 120.0°C
Die Temperature: 250 to 270.0°C
Drying Temperature: 100 to 110.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.