NORYL™ Resin PX1390 - Americas

Want to keep this datasheet? Save it now in your required format

Description

NORYL™ PX1390 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade inherently meets UL94 HB flame rating. NORYL PX1390 resin exhibits excellent electrical properties, easy processability, high heat resistance, and good dimensional stabilty. It is an excellent candidate for automotive connector applications.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Relative density

23.0 °C

1.06 [-]

Show Supplier Material materials with Relative density of 1.06 [-]

ASTM D 792

Water absorption

23.0 °C

0.1 %

Show Supplier Material materials with Water absorption of 0.1 %

ASTM D 570 | (23°C/24hrs)

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

30 %

Show Supplier Material materials with Elongation of 30 %

ASTM D 638 | brk, Type I, 50 mm/min

Flexural modulus

23.0 °C

2.27 GPa

Show Supplier Material materials with Flexural modulus of 2.27 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

99 MPa

Show Supplier Material materials with Flexural strength of 99 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Impact strength, Izod notched

23.0 °C

288 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 288 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

288 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 288 J/m

ASTM D 256

Tensile strength

23.0 °C

62 MPa

Show Supplier Material materials with Tensile strength of 62 MPa

ASTM D 638 | yld, Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

7.2E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7.2E-5 1/K

ASTM E 831 | 0°C to 100°C

Heat deflection temperature, 0.45 MPa

154 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C

ASTM D 648 | 6.4 mm, unannealed

Heat deflection temperature, 1.80 MPa

146 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 146 °C

ASTM D 648 | 6.4 mm, unannealed

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Gas/Electric Oven, Head Protection, Enclosures, Electronic Components, Data Transfer

Availability

Asia,Americas

Features

Hydrolytic Stability, Low Creep Sensitivity, High Heat Resistance, Good Stiffness, Low Warpage, Good Processability, Exceptional Processing

Processing methods

Mold Temperature: 75 to 105.0°C
Melt Temperature: 295 to 315.0°C
Drying Time: 3 to 4.0hrs
Shot to Cylinder Size: 30 to 70.0%
Back Pressure: 0.3 to 0.7MPa
Rear - Zone 1 Temperature: 260 to 305.0°C
Front - Zone 3 Temperature: 280 to 315.0°C
Nozzle Temperature: 295 to 315.0°C
Drying Temperature: 105 to 110.0°C
Maximum Moisture Content: 0.02%
Drying Time (Cumulative): 8hrs
Middle - Zone 2 Temperature: 270 to 310.0°C
Screw Speed: 20 to 100.0rpm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.