NORYL™ EN265 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high heat extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of v0 at 6mm and V1 at 1.5mm along with UL746C outdoor weatherability rating of F1. NORYL EN265 resin exhibits excellent impact strength, very low moisture absorption, good dimensional stability, and great machinability. NORYL EN185 resin is an excellent candidate for a variety of indoor and outdoor electrical applications including trunking and conduit.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Limiting oxygen index

23.0 °C

29.2 %

Show Supplier Material materials with Limiting oxygen index of 29.2 %

Relative density

23.0 °C

1.08 [-]

Show Supplier Material materials with Relative density of 1.08 [-]

ASTM D 792

Water absorption

23.0 °C

0.07 %

Show Supplier Material materials with Water absorption of 0.07 %

ASTM D 570 | (23°C/24hrs)

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

ASTM D 638 | brk, Type I, 50 mm/min

Flexural modulus

23.0 °C

2.55 GPa

Show Supplier Material materials with Flexural modulus of 2.55 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

99 MPa

Show Supplier Material materials with Flexural strength of 99 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Gardner Impact

23.0 °C

4 J

Show Supplier Material materials with Gardner Impact of 4 J

ASTM D 3029 | -40°C

Hardness, Rockwell R

23.0 °C

119 [-]

Show Supplier Material materials with Hardness, Rockwell R of 119 [-]

ASTM D 785

Impact strength, Izod notched

23.0 °C

186 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 186 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

186 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 186 J/m

ASTM D 256

Tensile strength

23.0 °C

63 MPa

Show Supplier Material materials with Tensile strength of 63 MPa

ASTM D 638 | yld, Type I, 50 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5.94E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.94E-5 1/K

ASTM E 831 | -40°C to 95°C

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

Glow Wire Ignition Temperature

725 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C

IEC 60695-2-13 | 2.0 mm

Heat deflection temperature

123 °C

Show Supplier Material materials with Heat deflection temperature of 123 °C

Heat deflection temperature, 1.80 MPa

123 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 123 °C

ASTM D 648 | 6.4 mm, unannealed

Relative temperature index, electrical

110 °C

Show Supplier Material materials with Relative temperature index, electrical of 110 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

110 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C

UL 746B

Flammability

UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Radiant Panel Listing: RP100- UL Tested <br> Glow Wire Flammability Index, 1.0 mm: 900°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 900°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 700°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 700°C IEC 60695-2-13 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221239- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

1 V

Show Supplier Material materials with Comparative tracking index of 1 V

UL 746A | (UL) {PLC}

Dielectric constant, 60Hz

23.0 °C

2.69 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.69 [-]

ASTM D 150 | 50/60 Hz

Dielectric strength

23.0 °C

19.6 kV/mm

Show Supplier Material materials with Dielectric strength of 19.6 kV/mm

ASTM D 149 | in oil, 3.2 mm

Dissipation factor, 50Hz

23.0 °C

7E-4 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 7E-4 [-]

ASTM D 150 | 50/60 Hz

High Amp Arc Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm

≥, UL 746A | PLC 0

High Volt Arc Track Rate

23.0 °C

4 PLC Code

Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code

UL 746A | (PLC)

Hot-Wire Ignition

23.0 °C

1.5 mm

Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm

≥, UL 746A | PLC 0

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Power Boat, Photovoltaic Components, Pharmaceutical Packaging & Drug Delivery, Building/Construction Sheet, Circuit Protection, Electronic Components, Enclosure/Housing/Cover, Heavy Vehicles

Availability

Americas

Features

Hydrolytic Stability, Flame Retardant, Non-Halogenated, Low Warpage

Processing methods

Melt Temperature: 225 to 255.0°C
Drying Temperature: 105 to 115.0°C
Die Temperature: 250°C
Barrel - Zone 3 Temperature: 225°C
Barrel - Zone 1 Temperature: 205°C
Adapter Temperature: 250°C
Barrel - Zone 2 Temperature: 205°C
Maximum Moisture Content: 0.02%
Drying Time (Cumulative): 8hrs
Drying Time: 2 to 4.0hrs
Barrel - Zone 4 Temperature: 225°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.