NORYL PPX™ Resin PPX7115 - Asia

Want to keep this datasheet? Save it now in your required format

Description

NORYL PPX™ 7115 resin is a non-reinforced alloy of polyphenylene ether (PPE) + polypropylene (PP). This injection moldable grade exhibits high modulus, high-temperature performance, excellent melt strength, impact resistance, hydrolytic and dimensional stability. NORYL PPX7115 resin is an excellent candidate for applications requiring high modulus and chemical resistance.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.37 GPa

Show Supplier Material materials with Elastic modulus of 1.37 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

75 %

Show Supplier Material materials with Elongation of 75 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

1.37 GPa

Show Supplier Material materials with Flexural modulus of 1.37 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural strength

23.0 °C

51 MPa

Show Supplier Material materials with Flexural strength of 51 MPa

ASTM D 790 | yld, 1.3 mm/min, 50 mm span

Impact strength, Izod notched

23.0 °C

534 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 534 kJ/m²

ASTM D 256 | notched, 23°C

Tensile strength

23.0 °C

35 MPa

Show Supplier Material materials with Tensile strength of 35 MPa

ISO 527 | yield, 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

112 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 112 °C

ASTM D 648 | 3.2 mm, unannealed

Heat deflection temperature, 1.80 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ASTM D 648 | 3.2mm, unannealed

Vicat softening temperature

131 °C

Show Supplier Material materials with Vicat softening temperature of 131 °C

ISO 306 | Rate A/50

Technological properties

Property
Application areas

Pipe/Fitting

Availability

Americas

Features

Hydrolytic Stability, Chemical Resistance, Low Creep Sensitivity, Low Warpage, High Impact Resistance

Processing methods

Drying Time: 2 to 4.0hrs
Drying Time (Cumulative): 8hrs
Melt Temperature: 260 to 290.0°C
Rear - Zone 1 Temperature: 225 to 275.0°C
Drying Temperature: 60 to 65.0°C
Screw Speed: 20 to 100.0rpm
Front - Zone 3 Temperature: 250 to 290.0°C
Maximum Moisture Content: 0.02%
Middle - Zone 2 Temperature: 240 to 280.0°C
Mold Temperature: 30 to 50.0°C
Nozzle Temperature: 260 to 290.0°C
Vent Depth: 0.038 to 0.051mm
Shot to Cylinder Size: 30 to 70.0%
Back Pressure: 0.3 to 0.7MPa

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.