ULTEM™ Resin HU1004 - Asia

Want to keep this datasheet? Save it now in your required format

Description

High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.28 g/cm³

Show Supplier Material materials with Density of 1.28 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

46 %

Show Supplier Material materials with Limiting oxygen index of 46 %

Relative density

23.0 °C

1.28 [-]

Show Supplier Material materials with Relative density of 1.28 [-]

ASTM D 792 |

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.9 GPa

Show Supplier Material materials with Elastic modulus of 2.9 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

80 %

Show Supplier Material materials with Elongation of 80 %

ISO 527 | break, 50 mm/min

Flexural modulus

23.0 °C

2.8 GPa

Show Supplier Material materials with Flexural modulus of 2.8 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

136 MPa

Show Supplier Material materials with Flexural strength of 136 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

11 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m²

ISO 179/2C | 23°C

Impact strength, Izod notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

70 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 70 J/m

ASTM D 256 | notched, 23°C

Instrumented Impact Ductility

23.0 °C

90 %

Show Supplier Material materials with Instrumented Impact Ductility of 90 %

ASTM D 3763 | -20°C

Instrumented Impact, Total Energy

23.0 °C

93 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 93 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

97 MPa

Show Supplier Material materials with Tensile strength of 97 MPa

ISO 527 | yield, 50 mm/min

Impact strength, Izod unnotched

ISO 180/1U | unnotched 80*10*4, -30°C

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

23.0 °C

5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Heat deflection temperature, 0.45 MPa

205 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C

ISO 75/Be | Edgew 120*10*4 sp=100mm

Heat deflection temperature, 1.80 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

105 °C

Show Supplier Material materials with Relative temperature index, electrical of 105 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

105 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B

Thermal conductivity

23.0 °C

0.19 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.19 W/(m·K)

ASTM C177

Vicat softening temperature

212 °C

Show Supplier Material materials with Vicat softening temperature of 212 °C

ISO 306 | Rate B/120

Flammability

UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 0.7- ASTM E 662 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100737020- -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm

≥, UL 746A | PLC 1

Hot-Wire Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm

≥, UL 746A | PLC 2

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

10 g/10min

Show Supplier Material materials with Melt mass-flow rate of 10 g/10min

ASTM D 1238 | 337°C/6.6 kgf

Melt volume-flow rate

14 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 14 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Animal Testing, Electronic Components, Enclosure/Housing/Cover, Lab Ware and Clinical Diagnostics, Surgical Devices, Renal and Blood Handling, Pharmaceutical Packaging & Drug Delivery, Medical Device, Medical Facility Infrastructure, Surgical Tray, Wire & cable

Availability

Europe,Asia,Americas

Features

Healthcare management of change, Steam, Gamma, EtO and E-beam sterilizable, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Steam Sterilizable, Gamma Sterilizable, E-beam Sterilizable, Food Contact Acceptable, Biocompatible

Processing methods

Mold Temperature: 130 to 160.0°C
Drying Time: 6 to 8.0hrs
Front - Zone 3 Temperature: 345 to 390.0°C
Maximum Moisture Content: 0.02%
Melt Temperature: 355 to 390.0°C
Back Pressure: 0.3 to 0.7MPa
Vent Depth: 0.025 to 0.076mm
Middle - Zone 2 Temperature: 335 to 390.0°C
Drying Time (Cumulative): 24hrs
Shot to Cylinder Size: 40 to 60.0%
Screw Speed: 40 to 70.0rpm
Drying Temperature: 150°C
Rear - Zone 1 Temperature: 330 to 390.0°C
Nozzle Temperature: 345 to 390.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.