ULTEM™ Resin DT1810EV - Europe

Want to keep this datasheet? Save it now in your required format

Description

Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.28 g/cm³

Show Supplier Material materials with Density of 1.28 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.08 %

Show Supplier Material materials with Moisture absorption of 0.08 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.28 [-]

Show Supplier Material materials with Relative density of 1.28 [-]

ASTM D 792 |

Water absorption

23.0 °C

0.36 %

Show Supplier Material materials with Water absorption of 0.36 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.5 GPa

Show Supplier Material materials with Elastic modulus of 2.5 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

80 %

Show Supplier Material materials with Elongation of 80 %

ISO 527 | break, 5 mm/min

Flexural modulus

23.0 °C

3.1 GPa

Show Supplier Material materials with Flexural modulus of 3.1 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

135 MPa

Show Supplier Material materials with Flexural strength of 135 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

2 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

2 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 2 kJ/m²

ISO 180/1A | notched 80*10*4, -30°C

Impact strength, Izod notched, ASTM

23.0 °C

32 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 32 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

48 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 48 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

98 MPa

Show Supplier Material materials with Tensile strength of 98 MPa

ISO 527 | yield, 5 mm/min

Impact strength, Izod unnotched, ASTM

ASTM D 4812 | unnotched, -30°C

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 5.5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Coefficient of thermal expansion, transverse

23.0 °C

5.5E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 5.5E-5 1/K

ISO 11359-2 | 23°C to 150°C

Glow Wire Flammability Index

960 °C

Show Supplier Material materials with Glow Wire Flammability Index of 960 °C

Glow Wire Ignition Temperature

825 °C

Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C

IEC 60695-2-13 | 3.0 mm

Heat deflection temperature, 1.80 MPa

168 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 168 °C

ISO 75/Ae | Edgew 120*10*4 sp=100mm

Relative temperature index, electrical

105 °C

Show Supplier Material materials with Relative temperature index, electrical of 105 °C

UL 746B

Relative temperature index, mechanical impact

105 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B

Relative temperature index, mechanical strength

105 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B

Vicat softening temperature

192 °C

Show Supplier Material materials with Vicat softening temperature of 192 °C

ISO 306 | Rate B/50

Flammability

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=640471- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

4 V

Show Supplier Material materials with Comparative tracking index of 4 V

UL 746A | (UL) {PLC}

High Amp Arc Ignition

23.0 °C

0.75 mm

Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm

≥, UL 746A | PLC 1

Hot-Wire Ignition

23.0 °C

3 mm

Show Supplier Material materials with Hot-Wire Ignition of 3 mm

≥, UL 746A | PLC 1

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

43 g/10min

Show Supplier Material materials with Melt mass-flow rate of 43 g/10min

ASTM D 1238 | 337°C/6.6 kgf

Melt volume-flow rate

56 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 56 cm³/10min

ISO 1133 | MVR at 360°C/5.0 kg

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Electronic Components, Data Transfer, Data Management, Personal Computing, Surgical Devices, Watch/Jewelry

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Enhanced Ductility, Chemical Resistance, Easy Flow, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant, Good Mold Release

Processing methods

Drying Temperature: 135°C
Drying Time: 4 to 6.0hrs
Drying Time (Cumulative): 12hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 330 to 355.0°C
Nozzle Temperature: 325 to 350.0°C
Front - Zone 3 Temperature: 330 to 355.0°C
Middle - Zone 2 Temperature: 320 to 345.0°C
Rear - Zone 1 Temperature: 310 to 330.0°C
Mold Temperature: 95 to 135.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 40 to 70.0rpm
Shot to Cylinder Size: 40 to 60.0%
Vent Depth: 0.025 to 0.076mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.