NORYL GTX™ Resin GTX944 - Asia

Want to keep this datasheet? Save it now in your required format

Description

NORYL GTX™ 944 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance along with improved processbility and increased impact performance. NORYL GTX944 resin may be an excellent candidate for Firefighter Helmet applications.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Supplier Material materials with Density of 1.07 g/cm³

ISO 1183

Limiting oxygen index

23.0 °C

21 %

Show Supplier Material materials with Limiting oxygen index of 21 %

Moisture absorption

23.0 °C

1.2 %

Show Supplier Material materials with Moisture absorption of 1.2 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.08 [-]

Show Supplier Material materials with Relative density of 1.08 [-]

ASTM D 792 |

Water absorption

23.0 °C

3.5 %

Show Supplier Material materials with Water absorption of 3.5 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2 GPa

Show Supplier Material materials with Elastic modulus of 2 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

3.5 %

Show Supplier Material materials with Elongation of 3.5 %

ISO 527 | yield, 50 mm/min

Flexural modulus

23.0 °C

1.9 GPa

Show Supplier Material materials with Flexural modulus of 1.9 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

75 MPa

Show Supplier Material materials with Flexural strength of 75 MPa

ISO 178 | yield, 2 mm/min

Hardness, Ball Indentation

23.0 °C

75 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 75 MPa

ISO 2039-1 | H358/30

Impact strength, Charpy notched

23.0 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C

Impact strength, Izod notched

23.0 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 25 kJ/m²

ISO 180/1A | 80*10*4, -30°C

Impact strength, Izod notched, ASTM

23.0 °C

680 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 680 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

55 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 55 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

45 MPa

Show Supplier Material materials with Tensile strength of 45 MPa

ISO 527 | break, 50 mm/min

Thermal

PropertyTemperatureValueComment

Ball Pressure Test

nan

IEC 60695-10-2 | 125°C +/- 2°C

Coefficient of thermal expansion

23.0 °C

9E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9E-5 1/K

ISO 11359-2 | 23°C to 60°C

Coefficient of thermal expansion, transverse

23.0 °C

9E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 9E-5 1/K

ISO 11359-2 | 23°C to 60°C

Heat deflection temperature, 0.45 MPa

175 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 175 °C

ISO 75/Be | Edgew 120*10*4 sp=100mm

Thermal conductivity

23.0 °C

0.24 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.24 W/(m·K)

ISO 8302

Vicat softening temperature

240 °C

Show Supplier Material materials with Vicat softening temperature of 240 °C

ISO 306 | Rate A/50

Flammability

UL Compliant, 94HB Flame Class Rating: 1.6mm UL 94 by SABIC-IP

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

IEC 60112 |

Dielectric constant, 1MHz

23.0 °C

2.7 [-]

Show Supplier Material materials with Dielectric constant, 1MHz of 2.7 [-]

IEC 60250

Dielectric constant, 60Hz

23.0 °C

3.5 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 3.5 [-]

IEC 60250 | 50/60 Hz

Dielectric strength

23.0 °C

20 kV/mm

Show Supplier Material materials with Dielectric strength of 20 kV/mm

IEC 60243-1 | in oil, 3.2 mm,

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-]

IEC 60250

Dissipation factor, 50Hz

23.0 °C

0.07 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 0.07 [-]

IEC 60250 | 50/60 Hz

Volume resistivity

23.0 °C

2.20E+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.20E+13 Ω·cm

IEC 60093 |

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

12.5 g/10min

Show Supplier Material materials with Melt mass-flow rate of 12.5 g/10min

ASTM D 1238 | 280°C/5.0 kgf

Melt volume-flow rate

12 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 12 cm³/10min

ISO 1133 | MVR at 280°C/5.0 kg

Shrinkage

23.0 °C

1.4 %

Show Supplier Material materials with Shrinkage of 1.4 %

SABIC method | 3.2 mm

Shrinkage, transverse

23.0 °C

1.1 %

Show Supplier Material materials with Shrinkage, transverse of 1.1 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Exterior, Heavy Vehicles, Head Protection, Enclosures, Electronic Components, Defense, Building Element

Availability

Europe

Features

Hydrolytic Stability, Chemical Resistance, Low Creep Sensitivity, Good Stiffness, Low Warpage, High Impact Resistance

Processing methods

Hopper Temperature: 60 to 80.0°C
Front - Zone 3 Temperature: 290 to 320.0°C
Drying Time: 2 to 3.0hrs
Nozzle Temperature: 280 to 310.0°C
Mold Temperature: 80 to 120.0°C
Melt Temperature: 290 to 320.0°C
Maximum Moisture Content: 0.07%
Middle - Zone 2 Temperature: 280 to 300.0°C
Drying Temperature: 100 to 120.0°C
Rear - Zone 1 Temperature: 260 to 280.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.