LEXAN™ Copolymer EXL4016H - Americas

Want to keep this datasheet? Save it now in your required format

Description

6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.22 g/cm³

Show Supplier Material materials with Density of 1.22 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.46 %

Show Supplier Material materials with Moisture absorption of 0.46 %

ISO 62 | (23°C / 50% RH)

Relative density

23.0 °C

1.22 [-]

Show Supplier Material materials with Relative density of 1.22 [-]

ASTM D 792 |

Water absorption

23.0 °C

0.12 %

Show Supplier Material materials with Water absorption of 0.12 %

ISO 62-1 | (23°C/saturated)

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.2 GPa

Show Supplier Material materials with Elastic modulus of 3.2 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

15.4 %

Show Supplier Material materials with Elongation of 15.4 %

ISO 527 | break, 5 mm/min

Flexural modulus

23.0 °C

2.83 GPa

Show Supplier Material materials with Flexural modulus of 2.83 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

104 MPa

Show Supplier Material materials with Flexural strength of 104 MPa

ISO 178 | yield, 2 mm/min

Impact strength, Charpy notched

23.0 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 25 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C

Impact strength, Izod notched

23.0 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 30 kJ/m²

ISO 180/1A | 80*10*3, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

166 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 166 J/m

ASTM D 256 | notched, -30°C

Instrumented Impact, Total Energy

23.0 °C

39 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 39 J

ASTM D 3763 | 23°C

Tensile strength

23.0 °C

47 MPa

Show Supplier Material materials with Tensile strength of 47 MPa

ISO 527 | break, 5 mm/min

Impact strength, Charpy unnotched

ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C

Impact strength, Izod unnotched

ISO 180/1U | unnotched 80*10*3, 23°C,

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

4.8E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.8E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

7.1E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 7.1E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

134 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 134 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Vicat softening temperature

146 °C

Show Supplier Material materials with Vicat softening temperature of 146 °C

ISO 306 | Rate B/50

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

6.6 g/10min

Show Supplier Material materials with Melt mass-flow rate of 6.6 g/10min

ASTM D 1238 | 300°C/1.2 kgf

Melt volume-flow rate

6 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 6 cm³/10min

ISO 1133 | MVR at 300°C/1.2 kg

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Enclosures

Availability

Europe,Asia,Americas

Features

High Impact Resistance

Processing methods

Drying Time: 3 to 4.0hrs
Rear - Zone 1 Temperature: 290 to 310.0°C
Screw Speed: 40 to 70.0rpm
Melt Temperature: 310 to 330.0°C
Middle - Zone 2 Temperature: 300 to 320.0°C
Mold Temperature: 80 to 115.0°C
Drying Time (Cumulative): 48hrs
Nozzle Temperature: 305 to 325.0°C
Front - Zone 3 Temperature: 310 to 330.0°C
Maximum Moisture Content: 0.02%
Drying Temperature: 120°C
Shot to Cylinder Size: 40 to 60.0%
Back Pressure: 0.3 to 0.7MPa
Vent Depth: 0.025 to 0.076mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.