Description

LNP THERMOCOMP WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.43 g/cm³

Show Supplier Material materials with Density of 1.43 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.2 %

Show Supplier Material materials with Elongation of 1.2 %

ISO 527 | yield

Flexural modulus

23.0 °C

17 GPa

Show Supplier Material materials with Flexural modulus of 17 GPa

ISO 178

Flexural strength

23.0 °C

219 MPa

Show Supplier Material materials with Flexural strength of 219 MPa

ISO 178

Impact strength, Izod notched

23.0 °C

4 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 4 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod unnotched

23.0 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 30 kJ/m²

ISO 180/1U | 80*10*4, 23°C

Tensile strength

23.0 °C

158 MPa

Show Supplier Material materials with Tensile strength of 158 MPa

ISO 527 | yield

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.23 %

Show Supplier Material materials with Shrinkage of 0.23 %

ISO 294 | 24 hrs

Technological properties

Property
Application areas

Lab Ware and Clinical Diagnostics, Semiconductor

Availability

Europe,Asia,Americas

Features

Super Strong (Carbon Fiber Filled), Structural

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.