LNP™ THERMOCOMP™ Compound RX06420 - Americas

Want to keep this datasheet? Save it now in your required format

Description

LNP THERMOCOMP RX06420 is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Low Extractable, Mold Release.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.29 g/cm³

Show Supplier Material materials with Density of 1.29 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

5.58 GPa

Show Supplier Material materials with Flexural modulus of 5.58 GPa

ISO 178 | 2 mm/min

Flexural strength

23.0 °C

179 MPa

Show Supplier Material materials with Flexural strength of 179 MPa

ASTM D 790

Impact strength, Izod notched

23.0 °C

50 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 50 kJ/m²

ASTM D 256 | notched, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

50 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

423 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 423 J/m

ASTM D 4812 | 23°C

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

221 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 221 °C

ASTM D 648 | 3.2mm, unannealed

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1 %

Show Supplier Material materials with Shrinkage of 1 %

ASTM D 955 | 24 hrs

Technological properties

Property
Application areas

Oil/Gas

Availability

Asia,Americas

Features

High Stiffness, Structural

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.