LNP™ STAT-KON™ Compound DEP32 - Europe

Want to keep this datasheet? Save it now in your required format

Description

LNP STAT-KON DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

7.8 GPa

Show Supplier Material materials with Elastic modulus of 7.8 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

2.6 %

Show Supplier Material materials with Elongation of 2.6 %

ISO 527 | break, 5 mm/min

Impact strength, Izod notched

23.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Tensile strength

23.0 °C

108 MPa

Show Supplier Material materials with Tensile strength of 108 MPa

ISO 527 | break, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

ISO 11359-2 | 23°C to 60°C

Coefficient of thermal expansion, transverse

23.0 °C

6.1E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.1E-5 1/K

ISO 11359-2 | 23°C to 60°C

Heat deflection temperature

141 - 145 °C

Show Supplier Material materials with Heat deflection temperature of 141 - 145 °C

Heat deflection temperature, 0.45 MPa

145 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 145 °C

ISO 75/Bf | Flatw 80*10*4 sp=64mm

Heat deflection temperature, 1.80 MPa

141 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 141 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Electrical

PropertyTemperatureValueComment

Sheet resistivity, ROA

23.0 °C

1000 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1000 Ω

ASTM D 257

Technological properties

Property
Application areas

ATM/Ticket Machine, Document Handling, Personal Computing

Availability

Europe,Americas

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.