ULTEM™ Resin AR9300 - Asia

Want to keep this datasheet? Save it now in your required format

Description

30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

8.96 GPa

Show Supplier Material materials with Elastic modulus of 8.96 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

3 %

Show Supplier Material materials with Elongation of 3 %

ASTM D 638 | brk, Type I, 5 mm/min

Flexural modulus

23.0 °C

9.65 GPa

Show Supplier Material materials with Flexural modulus of 9.65 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Flexural strength

23.0 °C

241 MPa

Show Supplier Material materials with Flexural strength of 241 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Tensile strength

23.0 °C

155 MPa

Show Supplier Material materials with Tensile strength of 155 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature

212 °C

Show Supplier Material materials with Heat deflection temperature of 212 °C

Heat deflection temperature, 1.80 MPa

212 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C

ASTM D 648 | 6.4 mm, unannealed

Flammability

NBS Smoke Density, Flaming, Dmax: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Ds 4 min: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Ds 1.5 min: 0- ASTM E 662 <br> OSU peak heat release rate (5 minute test): 40kW/m² FAR 25.853 <br> Vertical Burn a (60s) passes at: 0sec FAR 25.853 <br> Vertical Burn b (12s) passes at: 0sec FAR 25.853 <br> FAA Flammability, FAR 25.853 A/B: NATURAL- FAR 25.853

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 %

Show Supplier Material materials with Shrinkage of 0.2 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Enclosure/Housing/Cover, Air Cabin Interiors, Aircraft Seating, Aerospace

Availability

Europe,Asia,Americas

Features

High Stiffness, Hydrolytic Stability, Chemical Resistance, Low Smoke and Toxicity, Good Mechanicals in Broad Temperature Range, Low Creep Sensitivity, Low Shrinkage, Good metal adhesion, Amorphous, High Strength, High Heat Resistance, Good dimensional stability, Flame Retardant

Processing methods

Drying Time (Cumulative): 24hrs
Middle - Zone 2 Temperature: 355 to 375.0°C
Back Pressure: 0.3 to 0.7MPa
Rear - Zone 1 Temperature: 345 to 365.0°C
Drying Time: 4 to 6.0hrs
Mold Temperature: 135 to 165.0°C
Drying Temperature: 150°C
Front - Zone 3 Temperature: 365 to 390.0°C
Maximum Moisture Content: 0.02%
Vent Depth: 0.025 to 0.076mm
Screw Speed: 40 to 70.0rpm
Shot to Cylinder Size: 40 to 60.0%
Nozzle Temperature: 360 to 380.0°C
Melt Temperature: 365 to 390.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.