LNP™ THERMOTUF™ Compound IX02582 - Asia

Want to keep this datasheet? Save it now in your required format

Description

LNP THERMOTUF IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.41 g/cm³

Show Supplier Material materials with Density of 1.41 g/cm³

ASTM D 792

Moisture absorption

23.0 °C

0.28 %

Show Supplier Material materials with Moisture absorption of 0.28 %

ISO 62 | (23°C / 50% RH)

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

9.98 GPa

Show Supplier Material materials with Flexural modulus of 9.98 GPa

ISO 178 | 2 mm/min

Impact strength, Izod notched

23.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod notched, ASTM

23.0 °C

208 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 208 J/m

ASTM D 256 | notched, 23°C

Tensile strength

23.0 °C

157 MPa

Show Supplier Material materials with Tensile strength of 157 MPa

ISO 527 | break, 5 mm/min

Technological properties

Property
Application areas

Weapon

Availability

Asia,Americas

Features

High Stiffness, Structural

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.