ULTEM™ Foam XP080 - Americas

Want to keep this datasheet? Save it now in your required format

Description

ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The foam also possesses excellent dielectric properties. ULTEM foam is targeted at applications where structural fire performance, radar transparency, or extreme hot or cold environments are required. ULTEM foam is thermoformable and compatible with phenolic pre-pregs. Information on processing or secondary operations is available upon request.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.08 g/cm³

Show Supplier Material materials with Density of 0.08 g/cm³

ASTM D 1622

Mechanical

PropertyTemperatureValueComment

Compressive modulus, transverse

23.0 °C

71 MPa

Show Supplier Material materials with Compressive modulus, transverse of 71 MPa

ASTM D 1621

Compressive strength, transverse

23.0 °C

1.2 MPa

Show Supplier Material materials with Compressive strength, transverse of 1.2 MPa

ASTM D 1621

Elastic modulus

23.0 °C

0.04 GPa

Show Supplier Material materials with Elastic modulus of 0.04 GPa

ASTM D 638

Shear modulus

23.0 °C

0.02 GPa

Show Supplier Material materials with Shear modulus of 0.02 GPa

ASTM C 273

Shear strength

23.0 °C

1 MPa

Show Supplier Material materials with Shear strength of 1 MPa

ASTM C 273

Thermal

PropertyValue

Flammability

OSU peak heat release rate (5 minute test): <55kW/m² FAR 25.853 <br> Smoke Density: <10Ds FAR 25.853 <br> Smoke Toxicity: PASSES- OEM ABD <br> Vertical Burn at 60 Seconds: PASSES- FAR 25.853 <br> Insulation Radiant Panel: PASSES- FAR 25.856 <br> Smoke Toxicity: PASSES- OEM BSS

Technological properties

Property
Application areas

Sensor, Composite

Availability

Europe,Asia,Americas

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.