Cu-DHP (SF-Cu) Copper Hard

Want to keep this datasheet? Save it now in your required format

Description

Oxygen free copper grade

Equivalent Materials

This material data has been provided by Salomons Metalen.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Supplier Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

128 GPa

Show Supplier Material materials with Elastic modulus of 128 GPa

Elongation A5

23.0 °C

6 %

Show Supplier Material materials with Elongation A5 of 6 %

Hardness, Brinell

23.0 °C

102 [-]

Show Supplier Material materials with Hardness, Brinell of 102 [-]

Tensile strength

23.0 °C

420 MPa

Show Supplier Material materials with Tensile strength of 420 MPa

Yield strength Rp0.2

23.0 °C

320 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 320 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.76E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.76E-5 1/K

Thermal conductivity

23.0 °C

330 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 330 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

4.50E+7 S/m

Show Supplier Material materials with Electrical conductivity of 4.50E+7 S/m

Chemical properties

PropertyValue

Copper

99.9 %

Show Supplier Material materials with Copper of 99.9 %

Phosphorus

0.02 - 0.04 %

Show Supplier Material materials with Phosphorus of 0.02 - 0.04 %